Tarpaulin Specifications by GSM
This is the specification reference for TONGYUAN tarpaulin. It covers two materials: PE tarpaulin (60–300 GSM) and PVC tarpaulin (300 GSM upward). Look up a grade to see its construction, weight and tensile figures.
Where a value is not published, it is because we confirm the figure for your grade against the batch test report rather than print a generic number that may not match what ships. A specification that is wrong on the page costs more than one confirmed before the order.
Tarpaulin Specifications at a Glance
Two materials, each with its own construction, GSM range and test methods. Where a value is not published, it is because we confirm the figure for your grade against the batch test report rather than print a generic number that may not match what ships.
HDPE Woven + LDPE Coated
60–300 GSM. The woven tape carries the load; the LDPE coating on both sides makes the sheet waterproof. Heat-sealed or sewn seams.
Polyester Scrim + PVC Coating
300 GSM upward. Knife-coated or laminated, with high-frequency welded seams. The heavier, higher-cost, longer-life material of the two.
ASTM D751 & ISO 13934-1
Both materials are tested to the same methods, so the grade you specify is the grade you can verify. The exact figure is confirmed against the batch test report.
| Property | PE Tarpaulin | PVC Tarpaulin |
|---|---|---|
| Base fabric | HDPE woven tape | Polyester scrim |
| Coating | LDPE, both sides | PVC — knife-coated or laminated |
| GSM range | 60–300 GSM | 300 GSM upward |
| Seam | Heat-sealed or sewn | High-frequency welded |
| Tensile (published) | ~400 N/5cm at 120 GSM; ~650 at 180 GSM | Confirm per grade |
| Tear (published) | Confirm per grade | Confirm per grade |
| Test methods | ASTM D751, ISO 13934-1 | ASTM D751, ISO 13934-1 |
The two tensile figures above (~400 and ~650 N/5cm) are company-reported anchors for the middle of the PE range. The exact figure for a specific 150 GSM or 250 GSM grade is confirmed against the batch test report rather than estimated. Scroll horizontally on smaller screens.
On smaller screens, scroll horizontally to view all columns.
PE — 60–300 GSM
An HDPE woven fabric coated with LDPE on both sides. The woven tape carries the load; the coating makes the sheet waterproof. Light, medium and heavy duty grades within the range cover temporary covers through to truck covers and construction enclosure.
PVC — 300 GSM Upward
A polyester scrim with PVC coating, knife-coated or laminated. Fully waterproof and high-frequency welded, with the longest outdoor life of the two. Where a value is not published, it is confirmed per grade against the batch test report before the order.
Tarpaulin Specifications at a Glance
Two materials, each with its own construction, GSM range and test methods. Where a value is not published, it is because we confirm the figure for your grade against the batch test report rather than print a generic number that may not match what ships.
HDPE Woven + LDPE Coated
60–300 GSM. The woven tape carries the load; the LDPE coating on both sides makes the sheet waterproof. Heat-sealed or sewn seams.
Polyester Scrim + PVC Coating
300 GSM upward. Knife-coated or laminated, with high-frequency welded seams. The heavier, higher-cost, longer-life material of the two.
ASTM D751 & ISO 13934-1
Both materials are tested to the same methods, so the grade you specify is the grade you can verify. The exact figure is confirmed against the batch test report.
| Property | PE Tarpaulin | PVC Tarpaulin |
|---|---|---|
| Base fabric | HDPE woven tape | Polyester scrim |
| Coating | LDPE, both sides | PVC — knife-coated or laminated |
| GSM range | 60–300 GSM | 300 GSM upward |
| Seam | Heat-sealed or sewn | High-frequency welded |
| Tensile (published) | ~400 N/5cm at 120 GSM; ~650 at 180 GSM | Confirm per grade |
| Tear (published) | Confirm per grade | Confirm per grade |
| Test methods | ASTM D751, ISO 13934-1 | ASTM D751, ISO 13934-1 |
The two tensile figures above (~400 and ~650 N/5cm) are company-reported anchors for the middle of the PE range. The exact figure for a specific 150 GSM or 250 GSM grade is confirmed against the batch test report rather than estimated. Scroll horizontally on smaller screens.
On smaller screens, scroll horizontally to view all columns.
PE — 60–300 GSM
An HDPE woven fabric coated with LDPE on both sides. The woven tape carries the load; the coating makes the sheet waterproof. Light, medium and heavy duty grades within the range cover temporary covers through to truck covers and construction enclosure.
PVC — 300 GSM Upward
A polyester scrim with PVC coating, knife-coated or laminated. Fully waterproof and high-frequency welded, with the longest outdoor life of the two. Where a value is not published, it is confirmed per grade against the batch test report before the order.
PVC Tarpaulin Specifications
PVC tarpaulin is a polyester scrim coated with PVC — either knife-coated, where the PVC is fused into the weave, or laminated, where a PVC film is bonded onto the surface. It is the material buyers reach for when the cover has to be fully waterproof, weldable and long-lived.
Polyester scrim, PVC coating, high-frequency welded seams. Per-grade tensile, tear and temperature figures are confirmed for the specific grade — not published as one generic number.
- Knife-coated
- PVC fused into weave
- Laminated
- PVC film bonded to surface
- Seam
- High-frequency welded
- Treatments
- FR · UV · anti-mildew · anti-static · cold
Knife-Coated
300 GSM upward PVC fused into the polyester scrim Welds into a continuous seam
Laminated
300 GSM upward PVC film bonded onto a base fabric Lower cost at equal weight
Per-Grade, Not Generic
Tensile confirmed per grade Tear confirmed per grade Temperature confirmed per grade
What Is Fixed, and What Is Confirmed
What is fixed across the PVC range is the construction: polyester scrim, PVC coating, high-frequency welded seams, and treatment options that include flame retardancy, UV stabilisation, anti-mildew, anti-static and cold resistance. What is confirmed per grade — rather than published as a single generic number — is tensile, tear and temperature. That is deliberate: a specification that is wrong on the page costs more than one confirmed before the order.
PVC tarpaulin is the fully waterproof, weldable, long-life material of the range. For the full specification and treatment options, request the compliance pack or the batch test report for your grade.
How to Read a Tarpaulin Spec Sheet
A spec sheet only helps if the units are understood. These are the figures that appear on a tarpaulin specification, and what each one actually tells you.
Know What the Number Measures
GSM, N/5cm, N, °C and mm are different units measuring different properties. A heavier sheet is not automatically stronger, and a strong tensile does not prevent a tear.
Read Each Figure Against a Test
A number without a named method cannot be checked. ASTM D751, ISO 13934-1, ASTM D5034 and ASTM D4533 let you compare two spec sheets on the same property.
Ask If It Is Base or Finished
A “650 GSM” figure should be the finished, coated weight, not the raw scrim. Always ask which is quoted and put it on the order.
| Figure | What It Measures | What It Does Not Tell You |
|---|---|---|
| GSM grams per square metre | The weight of the fabric per square metre. PE runs 60–300 GSM; PVC starts around 300 GSM. Imperial equivalent is oz/yd² (1 oz/yd² ≈ 34 GSM). | Whether the sheet is stronger — a heavier sheet is generally stronger, not always. |
| Tensile N/5cm | The force needed to break a 5 cm-wide strip. Quoted as two numbers — warp (along the length) and weft (across the width). | Whether the weave resists a tear. Tensile and tear are different properties. |
| Tear strength N | Resistance to a tear that has already started — the kind that begins at an eyelet or a snag. | Breaking resistance of an intact strip. A fabric can be strong in tensile and still tear easily. |
| Temperature range °C | The span in which the material stays flexible rather than stiffening or embrittling. Grade-specific. | A single generic number — confirm it for the grade you are specifying. |
| Water resistance hydrostatic head | On PVC, how much water pressure the coated fabric withstands before leaking. Confirmed per grade. | Whether the seam leaks — a welded seam is tested separately. |
| Base vs finished weight | Which weight the figure refers to. Mostly a canvas trap, but it appears on coated fabrics too. | Anything, until you ask. Always confirm which is quoted and put it on the order. |
L = length; W = width not used here. Figures describe the property named, not the whole material — a spec sheet is read figure by figure, not as a single score. Scroll horizontally on smaller screens.
| Figure on the Sheet | Example · Spec Sheet Says | Confirmed Against the Test Report |
|---|---|---|
| 1. Read the unit | “650 GSM PVC” | Confirm it is finished coated weight, not raw scrim — a 50% difference on paper is common. |
| 2. Match to a method | Tensile quoted as “1,200 N/5cm” | Confirm the method — ASTM D751, ISO 13934-1, ASTM D5034. Same figure, different method, different meaning. |
| 3. Confirm base vs finished | Tear quoted as a single number | Ask for warp and weft separately. One number hides which direction was tested. |
| 4. Cross-check | Two sheets, same property | Compare the two figures against the same method — a higher number tested to a weaker method is not a stronger sheet. |
The most reliable way to read a spec sheet is to read it against a test report. Test methods such as ASTM D751, ISO 13934-1, ASTM D5034 and ASTM D4533 let you check the same property the same way on two different sheets.
Tensile and Tear Are Not the Same Property
Tensile measures breaking an intact strip; tear measures resistance to a tear that has already started — the kind that begins at an eyelet or a snag. A fabric can be strong in tensile and still tear easily, which is why eyelets and hems are reinforced.
Every Number Needs a Named Method
A spec sheet that quotes a figure without naming the test cannot be checked against another sheet or a test report. ASTM D751, ISO 13934-1, ASTM D5034 and ASTM D4533 are the standard set for coated and woven fabrics — ask for the method behind every number.
Choosing the Grade
GSM is the starting point, not the whole decision. Work from the application and the service life backwards to the grade, then confirm the tensile and tear against the test report. These grades are starting points, not rules.
Start With the Application
PE 60–100 GSM for light yard covers and temporary use. PE 120–180 GSM for equipment and storage. PE 150–250 GSM for hay, grain and silage. PE 200–300 GSM for truck covers on routine duty.
Step Up for Daily Duty
PVC 450–650 GSM for truck covers on daily exposed routes. PVC 500–650 GSM for tents and marquees. PVC 650 GSM upward for industrial and permanent installations.
Check the UV Package Too
In high-sun markets the UV stabiliser package affects service life more than the GSM does. Specify the treatment alongside the weight — a heavier sheet with a weak UV package can fail before a lighter sheet with a strong one.
Routine use on a trailer that is covered and uncovered a few times a week sits in PE 200–300 GSM. Once the route runs daily and the cover is exposed every day, the material moves to PVC 450–650 GSM — the same job, a heavier material, and a longer service life. The pattern is the point: capacity of use, not the size of the cover, decides the grade.
Tarpaulin GSM Guide
The full selection logic — which GSM for which job, and how to check it against the test report — has its own page. Use it to pin the grade once the application is fixed, and confirm the tensile and tear figures before the order.
Tarpaulin Material Guide
For the material-level decision between PE, PVC and canvas — waterproofing, breathability, service life and cost — the material guide compares them side by side, so the grade choice on this page starts from the right material.
Frequently Asked Questions
Answers about tensile strength, tear strength, GSM conversion, temperature range and how to verify a tarpaulin’s specifications.
What tensile strength is 200 GSM PE tarpaulin?
We publish ~400 N/5cm at 120 GSM and ~650 N/5cm at 180 GSM. For a specific 200 GSM grade we confirm the exact figure from the batch test report rather than print an estimated number — the value varies with the exact weave and coating, so the tested figure is the one that counts.
What is the difference between tensile strength and tear strength?
Tensile strength (N/5cm) is the force needed to break an intact 5 cm-wide strip. Tear strength (N) is the resistance to a tear that has already started — the kind that begins at an eyelet or a snag.
A fabric can be strong in one and weak in the other, which is why both are specified and tested.
What GSM is a 650 GSM PVC tarpaulin in ounces?
Roughly 19 oz/yd², using the 1 oz/yd² ≈ 34 GSM conversion.
oz/yd² ≈ GSM ÷ 34
The conversion is approximate. For a quoted grade, confirm the finished coated weight in both units against the spec sheet.
Is a higher GSM tarpaulin always stronger?
Usually, but not always. GSM measures weight, and a heavier sheet is generally stronger — but construction changes the result.
A woven scrim with a higher denier, or a different coating method, can be stronger at the same GSM. That is why tensile and tear are quoted separately from GSM.
What temperature can PVC tarpaulin withstand?
PVC stays flexible across a wide temperature range, but the exact rated span depends on the grade and the formulation.
Confirm the temperature range for the specific grade you are specifying, rather than applying a generic figure.
How do I verify a tarpaulin’s specifications before ordering?
Request the batch test report for the grade you are specifying. It records GSM, tensile, tear and the other tested properties to the same methods each time — ASTM D751, ISO 13934-1, ASTM D5034 and ASTM D4533.
Third-party inspection through BV or SGS is available on request.
The Specification That Matters Is on Your Batch Test Report
PE covers 60–300 GSM; PVC starts at 300 GSM upward, with per-grade figures confirmed for the grade rather than printed generically. Tell us the application, the GSM you are considering and the destination port — we will send the spec sheet and a sample so you can verify the figure before you commit to a container.